The physics in one paragraph
When a laser hits a particle, light bends around it. Big particles bend light through small angles. Small particles bend it through wide angles. Detectors collect the pattern, and software works backward to find the mix of sizes that would produce it. International standard ISO 13320 describes the method.
Our laser diffraction service measures particle size from 0.1 µm up to the coarse end of the range, so a single run covers ultra-fine powders and coarse granules.
Reading the result
- D50: the median. Half the volume is finer, half is coarser.
- D10: ten percent of the volume is finer than this.
- D90: ninety percent is finer than this. It tracks the coarse tail.
- Span: (D90 minus D10) divided by D50. A smaller span means a tighter distribution.
Example below: D10 near 14 µm, D50 near 32 µm, D90 near 71 µm.
Dry or wet?
In dry dispersion, compressed air carries the powder through the beam. It is fast and leaves nothing to clean. In wet dispersion, the powder is suspended in a liquid, often with ultrasound to break up clusters. Wet is gentler on fragile particles and handles very fine powders. The right method depends on the material.
Results are volume-based. A few large particles can dominate D90 even when they are rare by count. That is why D90 is useful for catching grit.
- Laser produces a stable, narrow beam.
- Sample cell. Powder is dispersed in a stream of air or in a liquid.
- Scattering. Big particles bend light a little, small particles bend it a lot.
- Detectors read the light pattern and software converts it to a size distribution.
Quick answers
Why use laser diffraction instead of sieves?
It gives a full distribution, works from sub-micron to millimeters, and takes minutes. Sieves are still useful as a simple check on the coarse end.
What is a good span?
There is no universal value. It depends on the product. The point is to keep it consistent lot to lot.